It was found that in the filling process, the material of option 1 is ABS-PC material, the total filling time is 0.9868s, the total filling time of scheme 2 is PC material, the total filling time is 1.004s, compared with the two, program 1 fill sfaster, material temperature is lower, the filling pressure is small, the combination line is not obvious, the gas hole is less.